HT-1769 UNITED ALLOY

categories

HT-1769 ULTRA WHITE CASTING PURPOSE

  • Brands United Alloys
  • Product Code: C1010321
  • Availability: In Stock
HT 1769 ULTRA WHITE CASTING PURPOSE CASTING technical data [PDF] United # HT-1769 White Alloy is formulated for 18 K white gold casting, giving a Ultra White color. The # HT-1769 White Alloys can also be used for continuous casting in 18 karat if desired.You should obtain excellent results by f...

HT 1769 ULTRA WHITE CASTING PURPOSE

CASTING technical data [PDF]

United # HT-1769 White Alloy is formulated for 18 K white gold casting, giving a Ultra White color. The # HT-1769 White Alloys can also be used for continuous casting in 18 karat if desired.

You should obtain excellent results by following a few simple instructions.

MELTING We do recommend pre-alloying all alloy and fine gold with aggressive stirring & fluxing to assure a uniform mixture.

Step : 1 Pre- Alloying (Fine gold + alloy) Temperature 1030° - 1050° C

1886° - 1922° F

Step : 2 Casting Temperature for 18 K Alloyed Grain 990° - 1010° C

1814° - 1850° F

FLASK TEMPERATURE Normal recommended temperature in the range of 580° C to 700° C / 1076° F – 1292° F depending on size of flask, karat & type of jewelry.

FLUXING Fluxing white gold is extremely important to pick-up oxides. Boric Acid is the recommended flux. Do not use carbon fluxes or any fluxes designed for refining; i.e., soda ash, saltpeter, etc. Avoid flux in bottom pour automatic casting units.